Compound Rubber SVR 3L & SBR 1502

Mixture of SVR 3L & SBR 1502

+ Demonstration of production process of mixture of SVR 3L & SBR 1502:

+ Current production capacity: 40 MT/day

+ Standard of mixture of SVR 3L and SBR 1502 follows TCVN 3769:2016 as basis

VIET NAM STANDARD 3769:2016 LIMIT
1. Dirt content (retained on 45µm aperture), % m/m, not more than 0.03
2. Ash content, % m/m, not more than 0.50
3. Nitrogen content, % m/m, not more than 0.60
4. Volatile content, % m/m, not more than 0.80
5. Initial plasticity (Po), not less than 35.0
6. Plasticity retention index (PRI), not less than 60.0
7. Color index (Lovibond), not less than 6